3DPrinting
3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.
The r/functionalprint community is now located at: or [email protected]
There are CAD communities available at: [email protected] or [email protected]
Rules
-
No bigotry - including racism, sexism, ableism, homophobia, transphobia, or xenophobia. Code of Conduct.
-
Be respectful, especially when disagreeing. Everyone should feel welcome here.
-
No porn (NSFW prints are acceptable but must be marked NSFW)
-
No Ads / Spamming / Guerrilla Marketing
-
Do not create links to reddit
-
If you see an issue please flag it
-
No guns
-
No injury gore posts
If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)
Moderation policy: Light, mostly invisible
view the rest of the comments
That was a typo, sorry, it was set at 195 C
All good! It's the same situation as I described and I see that increasing temps did help. It's good to do a temperature tower test for quality and also a full speed test after that. After temperature calibration, print a square that is only 2 or 3 bottom layers that covers the entire bed at full speed or faster. (It's essentially a combined adhesion/leveling/extrusion volume/z offset test, but you need to understand what you are looking at to see the issues separately.)
If you have extrusion problems, the layer line will start strong from the corners, get thin during the acceleration and may thicken up again at the bottom of the deceleration curve. A tiny bit of line width variation is normal, but full line separation needs attention.
Just be aware if you get caught in a loop of needing to keep bumping up temperatures as that starts to get into thermistor, heating element or even some mechanical issues/problems.