this post was submitted on 15 Jul 2023
7 points (100.0% liked)

3DPrinting

15595 readers
33 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I'm changing the PTFE in my heatbreak, I didn't realize these seem to be consumables. It started causing blockage.

A guy sent me a piece of PTFE from his Prusa MK3S+ that I could try as i was having trouble finding any PTFE quickly.

I realized I couldn't just cut a piece and put it in, that caused a lot of filament leakage and underextrusion. The end of the PTFE toward the nozzle was a bit jagged and I believe that's where the leakage happened. Now I'm wondering how the heatbreak and nozzle normally interface inside the heatblock, should they be touching? Should the PTFE protrude a bit from the heatbreak so there's a bit of pressure against the nozzle when I screw it in?

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 2 points 1 year ago

Yeah I've been printing a little PETG at about 240, but it's something I rarely do so I haven't opted for a all metal hotend and as I understood it I thought it was okay until about 250 C, but I guess not. It's really mostly PLA that I print though.

I'll look for a PTFE cutter, thanks!