this post was submitted on 28 Jan 2024
53 points (96.5% liked)

3DPrinting

15276 readers
63 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

Edit: Setting the max speed for walls to 50 mm/s solved it! I feel like this should be limited when you select the filament, but oh well.

Hey, so I have recently gotten a Bambu A1 and got a roll of PLA and PETG. The PLA is printing very nicely out of the box but the PETG not so much. Since I'm still very much at the beginning of my 3D printing journey, I don't really have a good way of drying my PETG yet, I just stuffed it in a plastic ziplock bag with all the desiccant bags I got from the rolls and printer and stored it that way. I'm already planning to print myself a filament enclosure, I just haven't gotten around to buying the bearings, etc for it.

I've done some functional prints with no angled (overhanging) walls and they have turned out pretty good. When printing on supports the overhangs are ugly af, but no weird pattern like this.

The issue I'm tracking down seems to occur on ~60+° overhangs, that really shouldn't be an issue. I've done a sliced test print and took some photos, any idea what causes this?
Thanks :)

Bambu A1, standard 0.4mm nozzle
Bambu PETG Basic filament and profile using Bambu Studio
Some settings I played around with was flow rate (0.94->0.95) and layer height (0.2mm -> 0.15mm) but it seems to make no difference.

(note, on some of them the part is photographed upside down.)

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 8 points 7 months ago (5 children)

Try slowing down your outer perimeter speed to 50mm/s and/or bump up your temperature by 10 degrees. Bambu's PETG defaults are bad IMO and my prints came out much better once I changed those two settings (the speed alone did it for me, but temp tower testing on Polymaker and Sunlu showed that higher temps printed nicer).

[–] [email protected] 4 points 7 months ago* (last edited 7 months ago)

I also figured out, I can adjust the max volumetric speed of the PETG filament settings and that will limit the wall speeds autumatically

Edit: This turned out to interact weirdly with layer height changes, I ended up just reducing the max speeds.